Julixing Instruments
 
Julixing Instruments

Company News

Test Probe Storage: Why Foam Inserts Fail After Five Years

Test Probe Storage: Why Foam Inserts Fail After Five Years

A probe kit arrives in a fitted foam insert. It looks like the right way to store precision tools, and for the first year it is. Five years later the foam has become the problem: it crumbles, it holds moisture against steel, and the probes show corrosion that nobody can explain.

What foam does over time

Three mechanisms, all slow:

Hydrolysis. Polyurethane foam absorbs water from the air and slowly breaks down. The reaction releases acids, which stay in the foam in contact with the tool.

Crumbling. The cell walls fracture, and the foam turns into a powder that coats every surface. That powder is mildly abrasive, and every time a probe is taken out and put back it works against the probe.

Compression set. The foam compresses where the probe rests and stops recovering. The probe then sits loose in a cavity that no longer holds it, and moves against the foam and against other probes.

Insert materialLifeRisk to the probe
polyurethane foam3 to 5 yearscrumbs, acid, moisture
cross-linked PE foamlongclosed cell, low shedding
machined PE blockvery longnone, but no cushioning

Why the probes get blamed

The corrosion that foam causes appears as fine pitting on the working surfaces, most often on the flanks of a thread or the barrel of a pin. It reads as a material or plating defect.

It is not. It is a probe that sat in an acid-loaded foam for years in an unheated store, and the pattern gives it away: the corrosion is heaviest on the surfaces that face down, because that is where the moisture collected.

The moisture trap

A closed case with foam in it is a humidity reservoir. The foam holds water, the case keeps it from escaping, and the temperature swings of a workshop drive the water in and out of the vapour phase against the steel.

The fix is not more foam. It is either a desiccant pack changed on a schedule, or a case that is not sealed, or both. A sealed case without desiccant is the worst of the options, because it holds whatever moisture was in the air on the day it was closed.

What to do in practice

Four actions, in the order they pay off:

Inspect the insert annually. Press it with a thumb. If it crumbles, or if it has left dust on a probe, replace it.

Replace with closed-cell foam or a machined insert. Cross-linked PE does not hydrolyse and does not shed. It cushions less, which matters for the thin probes and not at all for the thick ones.

Keep the probes oiled, not the foam dry. A thin film of protective oil on steel is the actual barrier. Foam condition is secondary.

Store cases off the floor and away from external walls. The coldest surface in a store is where condensation forms, and it is usually the wall or the floor.

The alternative that works better than any foam

Individual rigid tubes. A probe in its own tube cannot touch another probe, cannot be crushed by a heavy item placed on the case, and cannot sit in foam dust. The tube can be drilled at the base so that it drains rather than traps.

It is less convenient than a fitted case, which is exactly why fitted cases are used and why probes in fitted cases age faster than probes in tubes.

What to record

The insert type and its installation date, so that the age is known when a corrosion pattern appears. Two fields, and they turn an unexplained pitting finding into an explained one.

    Standard:       IEC 61032 IEC 60061 IEC 60335 IEC 60529 IEC 60068 IEC 60695 VDE 0620 UL AS/NZS3112
    TAG:
IEC Test Probe Go No Go Gauge Spring Impact Hammer Integrating Sphere UL Probe Test IP Tester Test Equipment
 
Glow Wire Tester Impact Test Hammer Go Gauge UL Test Finger Probe Hipot Tester Test Probe Needle Impact Testing Machine
  Español   Español Svenska   Svenska لعربية   لعربية русский   русский Português   Português China  中国 Polski   Polski Română   Română Dansk   Dansk suomi   suomi
  Français   Français hrvatski   hrvatski Ελληνικά   Ελληνικά Nederlands   Nederlands česky   česky Deutsch   Deutsch Japan   日本の Italia   Italia български   български นไทย   นไทย
test probe